3D Printer Under-Extrusion: 8 Simple Solutions

Last modified: August 12, 2022
You are here:
Estimated reading time: 4 min

Plagued by 3D printer under-extrusion and don’t know how to get rid of it? Check out this guide for some simple solutions.

Under-extrusion occurs when too little filament is extruded during a print. This can result in gaps, missing layers, insufficiently small layers, and even little dots or holes appearing in a print. Print quality and print strength are compromised when under-extrusion occurs.Under-extrusion can be either an issue related to settings and calibration (if you consistently experience under-extrusion) or it may have to do with hardware (if the issue suddenly arises). Make sure to check hardware issues first, and always be cautious of adjusting slicer settings too far if you’ve had successful prints in the past with the same setup.

In the following, we take a look at some easy fixes for under-extrusion that should eliminate this annoying problem. But before you begin, make sure you’ve got a favorite calibration cube or test print that you can use to dial in your settings.

Check Nozzle & Hot End

Step 1: Check your nozzle isn’t obstructed! (Source: Airwolf 3D)

The most common cause of under-extrusion is a clogged nozzle. Even just a partial clog can ruin your 3D prints. If your printer suddenly starts under-extruding, especially if you’ve been procrastinating on your printhead’s maintenance, a clogged nozzle is most likely the problem.

You can eliminate this issue by cleaning or replacing your printer’s nozzle. Most times, you can simply brush the nozzle with a wire brush and use an appropriately sized nozzle cleaner to push out leftover material and clear the nozzle opening. Other times, the solution is much more involved.

Check Bowden Tube & Cold End

Filament stuck in the Bowden tube can cause major problems (Source: Clever Creations)

If your nozzle is clean and you’re still experiencing under-extrusion, check your printer’s Bowden tube (or cold end if it’s a direct-drive setup). Sometimes, deteriorated PTFE tubing can fuse to filament and cause a clog.

To remove clogged filament and bad PTFE tubing, remove the collet clip, press down the collet around the PTFE tube, and give the tube a firm tug. It will also help to heat your hot end up to printing temperature (~200 °C), though be very careful if you choose this method. This will make sure filament isn’t stuck in the nozzle and will prevent removal of the Bowden tube.

If your printer has a direct drive extruder, you’ll need to access the cold end of the printhead to make sure filament can be pushed into the hot end without obstruction.

Check Extruder Gears

This extruder needs some proper cleaning (Source: LlamaLegend92 via Reddit)

A common cause of under-extrusion is uncleaned extruder gears. Especially if you’ve had clogging issues in the past, extruder gears can grind the stationary filament and accumulate filament shards and particles on the gear teeth. This will inhibit the extruder from gripping and pushing the filament through the nozzle.

A quick wire brushing should fix this issue for you in a jiffy!

Check for Filament Knots

Untangling filament knots can be a pain! (Source: Alec Richter via MatterHackers)

If you’ve checked all possible issues with your printer’s hardware, chances are you have a spool issue. Spool knots and tangles are annoyingly inevitable in your 3D printing journey. Be sure to check out our tips and tricks to avoid tangles.

The best way to fix a knot or tangle is to unwind your filament past the origin of the knot and carefully spool it back up. In the future, use a filament clip!

Increase Print Temperature

Temperature makes a huge difference! (Source: robomaniac via Thingiverse)

Even within the same material category, some filament brands and colors will require slightly different printing temperatures. If you recently switched filaments and are all-of-a-sudden seeing under-extrusion, chances are you need to adjust the print temperature. If the print temperature is too low, the filament won’t be able to flow properly.

Increase your print temperature by increments of 5 °C until you find the proper temperature for your machine and material. You can tweak this setting either by repeatedly printing a test and adjusting the temperature or by printing a single temperature tower, with which you can test several temperatures at once.

Adjust Retraction Settings

Poor retraction settings can cause gaps in a print (Source: Lord_Rexington via Reddit)

If you’re seeing under-extrusion near corners or seams of your prints, you might need to adjust your retraction settings. If you retract filament too far or too slowly, the extruder won’t be able to push enough filament through the nozzle to create a perfect layer.

Lower your retraction distance by 1 mm at a time and increase your retraction speed by 5 mm/s at a time. Stop when you see this issue disappear or become negligible. If your prints start stringing or blobs appear, you adjusted your distance and speed too much and need to backtrack a bit. As a general rule of thumb, never go below a 2-mm retraction distance or above ac 45-mm/s speed.

Correct Filament Diameter

This filament is slightly less than 1.75 mm in diameter (Source: Daniel VanBorkulo via YouTube)

This fix resolves a very common mistake: incorrect filament diameter input. As an extreme example, if your slicer is expecting 1.75-mm filament, and in fact, you’re trying to print with filament that’s 3 mm wide, the extruder won’t push the filament at a satisfactory rate.

Use calipers to measure your filament and find its correct diameter. Sometimes, even a 0.1-mm inaccuracy can cause printing issues.

Increase Flow Rate

Flow rate set to 80%, 96%, and 120% (Source: Teaching Tech)

If all your hardware is in tip-top shape, none of the settings tips are working, and you’re still experiencing under-extruded prints, try increasing the flow rate (also known as extrusion multiplier) in your slicer. This will push more filament through your nozzle resulting in fuller prints.

Tweak this setting by 2.5% until you find the right spot. Note, however, that increasing this setting too much can cause jamming. Sometimes different filament brands, colors, and materials will require slightly different flow rates. As a rule of thumb, don’t increase this setting to over 1.1 (or 110%). Otherwise, new problems will pop up.

As we noted before, never adjust this setting if you’ve produced acceptable prints with the same printer, settings, and material before. If under-extrusion randomly pops up, the issue is most likely in the hardware.

Source: https://all3dp.com/2/under-extrusion-3d-printing-all-you-need-to-know/